    廖友常. 一水硬铝石型高铁铝土矿的拜尔法溶出研究——以遵义仙人岩矿石为例[J]. 中国地质, 2012, 39(5): 1387-1396.
    引用本文: 廖友常. 一水硬铝石型高铁铝土矿的拜尔法溶出研究——以遵义仙人岩矿石为例[J]. 中国地质, 2012, 39(5): 1387-1396.
    LIAO You-chang. The Bayer dissolving method for the diaspore type high-iron bauxite: A case study of the ore from Xianrenyan rock in Zunyi[J]. GEOLOGY IN CHINA, 2012, 39(5): 1387-1396.
    Citation: LIAO You-chang. The Bayer dissolving method for the diaspore type high-iron bauxite: A case study of the ore from Xianrenyan rock in Zunyi[J]. GEOLOGY IN CHINA, 2012, 39(5): 1387-1396.

    一水硬铝石型高铁铝土矿的拜尔法溶出研究——以遵义仙人岩矿石为例

    The Bayer dissolving method for the diaspore type high-iron bauxite: A case study of the ore from Xianrenyan rock in Zunyi

    • 摘要: 提要:对于高铁铝土矿的应用,在以往的文献中,大多需先进行增铝降铁或铝、铁分离后才能利用。本文介绍了遵义仙人岩铝土矿床一水硬铝石型高铁铝土矿的物化特征,采集了含Al2O3 53.61% ,A/S 7.63 ,Fe2O3 21.96%的XCK5和Al2O351.71%, A/S 7.16, Fe2O3 24.89%的XCK4高铁铝土矿样,经拜尔法溶出试验,XCK5得到了绝对溶出率83.98%和相对溶出率96.65%,化学碱耗为57.9 kg(NaOH)/t(Al2O3);XCK4得到了绝对溶出率80.02%,相对溶出率93.01%,化学碱耗为34.9 kg(NaOH)/t(Al2O3);且赤泥沉降性能良好的试验结果。从而缩短了此类矿石需先进行增铝降铁或铝、铁分离后才能利用的工艺链,为该类矿石的应用和研究提供了一条新的途径。

       

      Abstract: Abstract:In the past, the adding of aluminum and reducing of iron or the separation of aluminum from iron should be adopted as the first step in the application of high iron bauxite, as indicated by most previous literatures. This paper describes physical and chemical characteristics of the diaspore type high iron bauxite in the ore bed of Xianrenyan Rock in Zunyi. The samples of XCK5 and XCK4 of high iron bauxite were collected, the former is characterized by Al2O3 53.61%,A/S 7.63,and Fe2O3 21.96%, whereas the latter is characterized by Al2O3 51.71%, A/S 7.16,and Fe2O3 24.89%. The Bayer dissolution test shows that the XCK5 has absolute dissolution rate 83.98% and relative dissolution rate 96.65%, chemical alkali consumption 57.9 kg(NaOH)/t(Al2O3), whereqs the XCK4 shows absolute dissolution rate 80.02%, relative dissolution rate 93.01%, and chemical alkali consumption 34.9 kg(NaOH)/t(Al2O3). The test also reaches good result in red mud settlement. Therefore, the process chain of the application of high iron bauxite can be considerably shortened in that it is not necessary to add aluminum and reduce iron or separate aluminum from iron first before the application. The result obtained by the authors provides a new way for this kind of ore applications and researches.

       

    /